Uns N02200 200 Nickel Pipe Pure Nickel Pipe Boiler Tube
Key Specifications / Features
Model no.: GWS-Pipe-976 Hits: 4
China Uns N02200 200 Nickel Pipe, Pure Nickel Pipe, Boiler Tube
Request a quote
share
Tags
Detail Information
Alloy 200/201 is extremely resistance to caustic alkalies up to and including the molten state. The extra-low carbon content of Alloy 200/201 gives virtual immunity to intergranular attack above about 315°C. The presence of chlorates must be kept to aminimum, as they accelerate the rate of attack.
Good resistance to corrosion in acids and alkalis and is most useful under reducing conditions.
Application
Alkali industry.
Chlor-alkali chemical and organic chloride production.
Food processing industry.
High temperature halogen and salt corrosion environment.
Electronic instrument parts. Water treatment.
Chemical
Product Parameters
Good resistance to corrosion in acids and alkalis and is most useful under reducing conditions.
Application
Alkali industry.
Chlor-alkali chemical and organic chloride production.
Food processing industry.
High temperature halogen and salt corrosion environment.
Electronic instrument parts. Water treatment.
Chemical
Grade | Ni+Co | Cu | Si | Mn | C | Mg | S | P |
N4 | 99.8 | 0.015 | 0.03 | 0.002 | 0.01 | 0.01 | 0.001 | 0.001 |
N6 | 99.6 | 0.10 | 0.10 | 0.05 | 0.10 | 0.10 | 0.005 | 0.002 |
Ni201 | ≥99.0 | ≤0.25 | ≤0.35 | ≤0.35 | ≤0.02 | / | ≤0.01 | / |
Ni200 | ≥99.2 | ≤0.25 | ≤0.35 | ≤0.35 | ≤0.15 | / | ≤0.01 | / |
Product Parameters
Physical Data | |||||
Density | Specific Heat | Electrical Resistivity | Melting Point | Thermal Conductivity | Mean Coeff Thermal Expansion |
8.89g/cm3 | 0.109(456 J/kg.ºC) | 0.096×10-6ohm.m | 1435-1446ºC | 70.2 W/m-K | 13.3×10-6m/m.ºC |
Typical Mechanical Properties | |||||
Mechanical Properties | Tensile Strength | Yield Strength | Elongation | Standard | |
Nickel 200 | 462 Mpa | 148 Mpa | 47% | ASTM B161/B163/B725/B751 |